{"id":38879,"date":"2017-08-31T09:57:14","date_gmt":"2017-08-31T07:57:14","guid":{"rendered":"https:\/\/www.sacome.com\/korrosion-verhindern-dichtungen-expansion\/"},"modified":"2025-10-01T10:14:28","modified_gmt":"2025-10-01T08:14:28","slug":"korrosion-verhindern-dichtungen-expansion","status":"publish","type":"post","link":"https:\/\/www.sacome.com\/de\/korrosion-verhindern-dichtungen-expansion\/","title":{"rendered":"Das Ph\u00e4nomen der Korrosion an Dichtungen"},"content":{"rendered":"<p>[et_pb_section bb_built=&#8220;1&#8243; admin_label=&#8220;section&#8220; parallax=&#8220;on&#8220; parallax_method=&#8220;off&#8220; _builder_version=&#8220;3.0.63&#8243; background_image=&#8220;https:\/\/www.sacome.com\/wp-content\/uploads\/2017\/08\/Evitar-la-corrosion-en-juntas-metalicas.jpg&#8220; next_background_color=&#8220;#ffffff&#8220;][et_pb_row admin_label=&#8220;row&#8220; custom_padding=&#8220;30px|0px|0px|0px&#8220; background_position=&#8220;&quot;&amp;quot;&amp;amp;quot;&amp;amp;amp;quot;top_left&amp;amp;amp;quot;&amp;amp;quot;&amp;quot;&quot;&#8220; background_repeat=&#8220;&quot;&amp;quot;&amp;amp;quot;&amp;amp;amp;quot;repeat&amp;amp;amp;quot;&amp;amp;quot;&amp;quot;&quot;&#8220; background_size=&#8220;&quot;&amp;quot;&amp;amp;quot;&amp;amp;amp;quot;initial&amp;amp;amp;quot;&amp;amp;quot;&amp;quot;&quot;&#8220;][et_pb_column type=&#8220;4_4&#8243;][et_pb_blurb admin_label=&#8220;Blurb&#8220; animation=&#8220;bottom&#8220; text_orientation=&#8220;center&#8220; background_position=&#8220;top_left&#8220; background_repeat=&#8220;repeat&#8220; background_size=&#8220;initial&#8220; _builder_version=&#8220;3.0.63&#8243; url_new_window=&#8220;off&#8220; use_icon=&#8220;off&#8220; use_circle=&#8220;off&#8220; use_circle_border=&#8220;off&#8220; icon_placement=&#8220;top&#8220; use_icon_font_size=&#8220;off&#8220; background_layout=&#8220;light&#8220; border_style=&#8220;solid&#8220; image_max_width=&#8220;100%&#8220; \/][\/et_pb_column][\/et_pb_row][et_pb_row admin_label=&#8220;row&#8220; custom_padding=&#8220;0px|0px|0px|0px&#8220; background_position=&#8220;&quot;&amp;quot;&amp;amp;quot;&amp;amp;amp;quot;top_left&amp;amp;amp;quot;&amp;amp;quot;&amp;quot;&quot;&#8220; background_repeat=&#8220;&quot;&amp;quot;&amp;amp;quot;&amp;amp;amp;quot;repeat&amp;amp;amp;quot;&amp;amp;quot;&amp;quot;&quot;&#8220; background_size=&#8220;&quot;&amp;quot;&amp;amp;quot;&amp;amp;amp;quot;initial&amp;amp;amp;quot;&amp;amp;quot;&amp;quot;&quot;&#8220;][et_pb_column type=&#8220;4_4&#8243;][et_pb_text admin_label=&#8220;Text&#8220; background_layout=&#8220;dark&#8220; text_orientation=&#8220;center&#8220; background_position=&#8220;top_left&#8220; background_repeat=&#8220;repeat&#8220; background_size=&#8220;initial&#8220; _builder_version=&#8220;3.17.6&#8243; border_style=&#8220;solid&#8220; module_alignment=&#8220;center&#8220;]<\/p>\n<h2 style=\"font-size: 44px; font-weight: 300;\">Korrosionsangriff auf metallische Dehnungsdichtungen<\/h2>\n<p>[\/et_pb_text][\/et_pb_column][\/et_pb_row][\/et_pb_section][et_pb_section bb_built=&#8220;1&#8243; fullwidth=&#8220;off&#8220; specialty=&#8220;off&#8220; prev_background_color=&#8220;#000000&#8243; next_background_color=&#8220;#000000&#8243;][et_pb_row][et_pb_column type=&#8220;4_4&#8243;][et_pb_text _builder_version=&#8220;3.17.6&#8243; border_style=&#8220;solid&#8220;]<\/p>\n<h2 style=\"text-align: center;\">Ursachen f\u00fcr Korrosion an metallischen Kompensatoren<\/h2>\n<p style=\"text-align: justify;\">Die Lebensdauer eines <a href=\"https:\/\/www.deepl.com\/?page_id=1176\"><b>metallischen Kompensators<\/b><\/a> oder <b>metallischen Dehnungsausgleichers<\/b> kann durch <b>Korrosion<\/b> erheblich verk\u00fcrzt werden. Die Konstruktion und die Betriebseigenschaften metallischer Kompensatoren sind so beschaffen, dass sie unter Bedingungen, die Rohrleitungen oder Befestigungen aus \u00e4hnlichen Werkstoffen nicht beeintr\u00e4chtigen, einem <b>korrosiven Angriff<\/b> ausgesetzt sein k\u00f6nnen.<\/p>\n<p>&nbsp;<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-3991 size-full\" title=\"Junta de expansi\u00f3n met\u00e1lica universal con tirantes.\" src=\"https:\/\/www.sacome.com\/wp-content\/uploads\/2017\/08\/Galeria-Compensador-de-Dilatacion-Universal-SACOME_6.jpg\" alt=\"Compensador de dilataci\u00f3n met\u00e1lico universal con tirantes.\" width=\"500\" height=\"500\" srcset=\"https:\/\/www.sacome.com\/wp-content\/uploads\/2017\/08\/Galeria-Compensador-de-Dilatacion-Universal-SACOME_6.jpg 500w, https:\/\/www.sacome.com\/wp-content\/uploads\/2017\/08\/Galeria-Compensador-de-Dilatacion-Universal-SACOME_6-150x150.jpg 150w, https:\/\/www.sacome.com\/wp-content\/uploads\/2017\/08\/Galeria-Compensador-de-Dilatacion-Universal-SACOME_6-300x300.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p>&nbsp;<\/p>\n<p style=\"text-align: justify;\">Die h\u00e4ufigsten <b>Arten von Korrosion<\/b> an <b>metallischen Dehnungsdichtungen<\/b> oder Kompensatoren sind folgende:<\/p>\n<ul style=\"text-align: justify;\">\n<li><b>Spannungskorrosion<\/b>, die sich durch einen Materialbruch infolge einer Kombination aus Spannungen und einem korrosiven Medium \u00e4u\u00dfert.<\/li>\n<li><b>Interkristalline Korrosion<\/b>, die durch einen bevorzugten Angriff \u00fcber die Korngrenzen der Werkstoffe hinweg gekennzeichnet ist.<\/li>\n<li><b>Pitting<\/b>, ein lokaler Angriff auf Metalle.<\/li>\n<li><b>Allgemeine Korrosion<\/b> oder allm\u00e4hliche Zersetzung von Metallen in einem System.<\/li>\n<li><b>Erosion unter Korrosion<\/b>, verbunden mit dem Aufprall einer fl\u00fcssigen oder gasf\u00f6rmigen Umgebung auf die Oberfl\u00e4che des angegriffenen Materials.<\/li>\n<\/ul>\n<p style=\"text-align: justify;\">\n<blockquote><p><strong>Die Oxidation bei hohen Temperaturen ist eine weitere Form der Materialzerst\u00f6rung, die sehr h\u00e4ufig in Hei\u00dfluft und Abgasleitungen auftritt..<\/strong><\/p><\/blockquote>\n<p>&nbsp;<\/p>\n<p style=\"text-align: justify;\"><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-5528 alignleft\" title=\".El fen\u00f3meno de corrosi\u00f3n en juntas de expansi\u00f3n.\" src=\"https:\/\/www.sacome.com\/wp-content\/uploads\/2017\/08\/Evitar-la-corrosion-en-juntas-metalicas-1024x683.jpg\" alt=\"La resistencia a la corrosi\u00f3n del acero inoxidable depende de la formaci\u00f3n de una capa delgada, sin roturas, de \u00f3xido de cromo, que se formar\u00e1 lentamente en la atm\u00f3sfera sobre el acero inoxidable limpio.\" width=\"500\" height=\"333\" srcset=\"https:\/\/www.sacome.com\/wp-content\/uploads\/2017\/08\/Evitar-la-corrosion-en-juntas-metalicas-1024x683.jpg 1024w, https:\/\/www.sacome.com\/wp-content\/uploads\/2017\/08\/Evitar-la-corrosion-en-juntas-metalicas-300x200.jpg 300w, https:\/\/www.sacome.com\/wp-content\/uploads\/2017\/08\/Evitar-la-corrosion-en-juntas-metalicas-768x512.jpg 768w, https:\/\/www.sacome.com\/wp-content\/uploads\/2017\/08\/Evitar-la-corrosion-en-juntas-metalicas-610x407.jpg 610w, https:\/\/www.sacome.com\/wp-content\/uploads\/2017\/08\/Evitar-la-corrosion-en-juntas-metalicas-1080x720.jpg 1080w, https:\/\/www.sacome.com\/wp-content\/uploads\/2017\/08\/Evitar-la-corrosion-en-juntas-metalicas.jpg 1200w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p style=\"text-align: justify;\">Das Auftreten jeder Korrosionsart h\u00e4ngt von der Art und den Eigenschaften des jeweiligen Materials sowie von den Ausgangsbedingungen seiner Oberfl\u00e4che ab. Die Auswahl des Werkstoffs muss so erfolgen, dass keine Korrosion auftreten kann oder dass die Korrosion nicht \u00fcber eine Eindringtiefe von 0,002 Zoll pro Jahr hinausgeht. Die <b>Korrosionsbest\u00e4ndigkeit von Edelstahl<\/b> h\u00e4ngt von der Bildung einer d\u00fcnnen, ununterbrochenen Schicht aus <b>Chromoxid<\/b> ab, die sich langsam in der Atmosph\u00e4re auf sauberem Edelstahl bildet. Stahlpartikel, wie z. B. Schwei\u00dfspritzer, verhindern die Bildung dieser Chromoxidschicht. Um eine maximale allgemeine Korrosionsbest\u00e4ndigkeit zu erreichen, sollten daher alle Zunder durch Beizen entfernt werden. Das Anhaften von Schwei\u00dfspritzern sollte sowohl bei der Lagerung als auch bei der Installation durch Abdecken der Faltenb\u00e4lge oder durch Verwendung einer Spritzschutzmasse vermieden werden. Obwohl es manchmal ratsam ist, austenitische Edelstahlkomponenten von Rohrleitungen zu erw\u00e4rmen, um ihre Korrosionsbest\u00e4ndigkeit zu verbessern, ist dies bei Faltenb\u00e4lgen nicht \u00fcblich.<\/p>\n<p style=\"text-align: justify;\">\n<p style=\"text-align: justify;\">Bei der <b>Konstruktion von Rohrleitungssystemen<\/b> mit metallischen Kompensatoren muss nicht nur den inneren, sondern auch den \u00e4u\u00dferen Bedingungen besondere Aufmerksamkeit geschenkt werden. In der Praxis lassen sich viele Korrosionsprobleme mit Hilfe einer <b>gut geplanten Studie<\/b>, die die <b>richtige Konstruktion<\/b> ermittelt, erheblich reduzieren. Der Konstrukteur oder Ingenieur muss Situationen vorhersehen, in denen es aufgrund einer fehlerhaften Konstruktion oder einer ungeeigneten Materialauswahl zu <b>Korrosionsangriffen<\/b> kommen kann. Da <b>Korrosionsprobleme<\/b> komplex sein k\u00f6nnen, ist es ratsam, sich an <b>Materialingenieure<\/b> zu wenden, wie sie beispielsweise in der Qualit\u00e4tsabteilung von <b>SACOME<\/b> t\u00e4tig sind.<\/p>\n<p>&nbsp;<\/p>\n<p>[\/et_pb_text][\/et_pb_column][\/et_pb_row][\/et_pb_section][et_pb_section bb_built=&#8220;1&#8243; fullwidth=&#8220;off&#8220; specialty=&#8220;off&#8220; prev_background_color=&#8220;#000000&#8243;][et_pb_row][et_pb_column type=&#8220;4_4&#8243;][et_pb_blog _builder_version=&#8220;3.17.6&#8243; posts_number=&#8220;3&#8243; include_categories=&#8220;34&#8243; show_author=&#8220;off&#8220; show_date=&#8220;off&#8220; show_pagination=&#8220;off&#8220; fullwidth=&#8220;off&#8220; use_overlay=&#8220;on&#8220; hover_overlay_color=&#8220;rgba(0,0,0,0.44)&#8220; header_level=&#8220;h3&#8243; \/][\/et_pb_column][\/et_pb_row][\/et_pb_section]<\/p>\n","protected":false},"excerpt":{"rendered":"<p>Korrosion an metallischen Dehnungsdichtungen kann die Lebensdauer des Kompensators erheblich verk\u00fcrzen. Die Konstruktion und die Betriebseigenschaften von Dehnungsdichtungen sind so beschaffen, dass sie unter Bedingungen, die Rohrleitungen oder Befestigungen aus \u00e4hnlichen Werkstoffen nicht beeintr\u00e4chtigen, korrosiv angegriffen werden k\u00f6nnen.<\/p>\n","protected":false},"author":2,"featured_media":38881,"comment_status":"closed","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[228],"tags":[],"class_list":["post-38879","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-technische-dokumentation-kompensatoren"],"_links":{"self":[{"href":"https:\/\/www.sacome.com\/de\/wp-json\/wp\/v2\/posts\/38879"}],"collection":[{"href":"https:\/\/www.sacome.com\/de\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.sacome.com\/de\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.sacome.com\/de\/wp-json\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"https:\/\/www.sacome.com\/de\/wp-json\/wp\/v2\/comments?post=38879"}],"version-history":[{"count":1,"href":"https:\/\/www.sacome.com\/de\/wp-json\/wp\/v2\/posts\/38879\/revisions"}],"predecessor-version":[{"id":38882,"href":"https:\/\/www.sacome.com\/de\/wp-json\/wp\/v2\/posts\/38879\/revisions\/38882"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.sacome.com\/de\/wp-json\/wp\/v2\/media\/38881"}],"wp:attachment":[{"href":"https:\/\/www.sacome.com\/de\/wp-json\/wp\/v2\/media?parent=38879"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.sacome.com\/de\/wp-json\/wp\/v2\/categories?post=38879"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.sacome.com\/de\/wp-json\/wp\/v2\/tags?post=38879"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}